| ==== The head consists of the following printed parts: ==== | ==== The head consists of the following printed parts: ==== | ||
| - | * Front shell (gas mask) | + | * Front shell (gas mask){{: |
| - | * Back shell | + | * Back shell{{: |
| * Backplate | * Backplate | ||
| * Adapters for the " | * Adapters for the " | ||
| Line 66: | Line 66: | ||
| You may need to repeat one or more of these steps (especially during sanding) depending on the print, and how fine of a finish you'd like. | You may need to repeat one or more of these steps (especially during sanding) depending on the print, and how fine of a finish you'd like. | ||
| + | |||
| + | Print settings for LW-PLA I used (on modified CR-10S with a microswiss direct drive extruder): | ||
| + | * Extrusion multiplier: 0.52 | ||
| + | * Print temperature: | ||
| + | * Print speed: 50 mmm/s | ||
| + | * Retract distance: 0.5 mm | ||
| + | * Retract as few times and as little as possible, otherwise the hotend may clog! | ||
| + | * Wall loops: 3 | ||
| + | * Infill: 10 % rectilinear | ||
| + | * 4 top and 4 bottom shells | ||
| + | * Layer height: 0.2 mm | ||
| + | |||
| ==== Ears ==== | ==== Ears ==== | ||
| Line 74: | Line 86: | ||
| This resulted in ears that are under 100 grams each, which made a huge difference in comfort. | This resulted in ears that are under 100 grams each, which made a huge difference in comfort. | ||
| + | Printing LW-TPU can be a bit tricky as I learned. It has to be printed very slowly, and it sticks to the build plate extremely strongly, so it has to be removed carefully. | ||
| + | |||
| + | Print settings (on direct drive CR-10S): | ||
| + | * Extrusion multiplier: 0.6 | ||
| + | * Retract distance: 3 mm | ||
| + | * Retract speed: 35 mm/s | ||
| + | * Coast to end enabled, distance: 5 mm | ||
| + | * Layer height: 0.2 mm | ||
| + | * Wall loops: 2 (depends on the parts, the bottom part, up to the hole, has 3 perimeters with 0.4 mm nozzle, 2 with 0.6 mm nozzle, but above that only 2 (this stays 2 for the 0.6 mm nozzle as well unfortunately) | ||
| + | * Print temperature: | ||
| + | * Bed temperature: | ||
| + | * Part cooling fan : 50 % | ||
| + | * Printing speed: 40 mm/s (with the 0.6 mm nozzle this is too fast, especially for vase mode, had to halve it to 20 mm/s) | ||
| + | * Reduction of print speed for short layer times was enabled (otherwised the ear tips would go melty), was set to 5 sec, with a minimum speed of 5 % | ||